Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.20e+14 ohm-cm | 2.20e+14 ohm-cm | 150°C for 1,000 hrs; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-Hb Gap Filler Pad Sarcon GR-b is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Volume Resistivity | 2.20e+14 ohm-cm | 2.20e+14 ohm-cm | ASTM D257 |
3M Scotch-Weld™ DP-100NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP-100NS is a two-part adhesives offering fast cure and machinability.Information provided by 3M |