Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.20e+12 ohm-cm | 2.20e+12 ohm-cm | ASTM D247 |
Plenco 2300 Phenolic, Granular, Compression Molded PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654.. |
|||
Volume Resistivity | 2.20e+12 ohm-cm | 2.20e+12 ohm-cm | ASTM D247 |
Plenco 3597 Phenolic, Granular, Injection Molded PLENCO 03597 is a mineral filled phenolic molding compound offering excellent flammability ratings even at thin cross sections, along with excellent arc and comparative track resistance values. UL r.. |
|||
Volume Resistivity | 2.20e+12 ohm-cm | 2.20e+12 ohm-cm | ASTM D257 |
3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |