Polymer Property : Volume Resistivity = 1e+16 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1e+15 - 1e+16 ohm-cm
1e+15 - 1e+16 ohm-cm
ASTM D257
Kureha KF Polymer 1100 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Volume Resistivity 1e+15 - 1e+16 ohm-cm
1e+15 - 1e+16 ohm-cm
ASTM D257
Kureha KF Polymer 850 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Volume Resistivity 1e+15 - 1e+16 ohm-cm
1e+15 - 1e+16 ohm-cm
ASTM D257
Kureha KF Polymer 1000 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Volume Resistivity 1e+15 - 1e+16 ohm-cm
1e+15 - 1e+16 ohm-cm
ASTM D257
Kureha KF Polymer 1300 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Volume Resistivity 1e+15 - 1e+16 ohm-cm
1e+15 - 1e+16 ohm-cm
ASTM D257
Kureha KF Polymer 2950 PVDF Copolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..