Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Volume Resistivity = 1e+15 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1e+15 - 1e+16 ohm-cm
1e+15 - 1e+16 ohm-cm
ASTM D257
Kureha KF Polymer 1100 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Volume Resistivity 1e+15 - 1e+16 ohm-cm
1e+15 - 1e+16 ohm-cm
ASTM D257
Kureha KF Polymer 850 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Volume Resistivity 1e+15 - 1e+16 ohm-cm
1e+15 - 1e+16 ohm-cm
ASTM D257
Kureha KF Polymer 1000 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Volume Resistivity 1e+15 - 1e+16 ohm-cm
1e+15 - 1e+16 ohm-cm
ASTM D257
Kureha KF Polymer 1300 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Volume Resistivity 1e+15 - 1e+16 ohm-cm
1e+15 - 1e+16 ohm-cm
ASTM D257
Kureha KF Polymer 2950 PVDF Copolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Volume Resistivity >= 1e+15 ohm-cm

@Temperature 25.0 °C
>= 1e+15 ohm-cm

@Temperature 77.0 °F
Master Bond MB250NT Low viscosity ethyl cyanoacrylate
Master Bond MB250NT is a single component ethyl cyanoacrylate type system. This rapid curing, high strength system is used primarily in applications where the ISO 10993-5 for low toxicity is specifi..
Volume Resistivity >= 1e+15 ohm-cm
>= 1e+15 ohm-cm
Master Bond Super Gel 9 Two component urethane modified epoxy gel-like system
Cures at room temperature to form a soft, resilient gel-like system with good dimensional stability. It has excellent optical clarity, convenient to handle, and is easy to retrieve with a sharp kni..
Copyright © lookpolymers.com All Rights Reserved