Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boil.. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® 3400 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3400 polyethersulfone (PESU) is a high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boi.. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral acids... |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn.. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to st.. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU) Veradel® 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, .. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU) Veradel® 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel® 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensi.. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac.. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® 3300 ULT Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability as well as resistance to steam, hot water and mineral a.. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® 3400 Polyethersulfone (PESU) Veradel® 3400 polyethersulfone (PESU) is a high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam,.. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac.. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU) Veradel® 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to s.. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU) Veradel® A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance t.. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU) Veradel® A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance.. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral aci.. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D247 |
Plenco 1581 Polyester, Pellet, Injection Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Westlake Plastics Polyethersulfone High resistance to heat and combustibility, low smoke emission, and transparency are the combination of properties possessed by stock shapes extruded from PES. These, coupled with light weight, good.. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | |
ACC QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber QSil 216 is a two-part, clear, liquid silicone which will cure at room temperature or at elevated temperatures. It has a low viscosity, which allows for ease of flow around complex parts, providing .. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensional sta.. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and .. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance to .. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. .. |
|||
Volume Resistivity | 1.70e+15 ohm-cm | 1.70e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® 3300 Polyethersulfone (PESU)
(discontinued **) Veradel 3300 polyethersulfone (PESU) is a medium melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, b.. |