Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.22e+16 ohm-cm | 1.22e+16 ohm-cm | "A" |
Abatron AboCast 8501-6 One-Component Epoxy AboCast 8501-6 is a clear, high-temperature one-component epoxy system for very high-temperature uses. It offers the highest heat resistance of the clear resins. Suggested Uses: Casting; Potting; E.. |
|||
Volume Resistivity | 1.22e+16 ohm-cm | 1.22e+16 ohm-cm | C 96/23/96 |
Abatron AboCast 8504-1 One-Component Epoxy AboCast 8504-1 is a clear, all-purpose one-component epoxy system, with an optimum balance of properties for most casting, adhesive, impregnation, and coating applications. |