Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.0e+13 ohm-cm | >= 1.0e+13 ohm-cm | IEC 60093 |
Quadrant EPP Acetron® MD POM-C + metal detectable additive, extruded (ISO Data) Metal detectable POM-C grade High mechanical strength, stiffness and hardness Excellent resilience Good creep resistance High impact strength, even at low temperatures Very good dimensional stabilit.. |
|||
Volume Resistivity | >= 1.0e+13 ohm-cm | >= 1.0e+13 ohm-cm | IEC 60093 |
Quadrant EPP Duratron® PAI T4301 PAI + graphite + PTFE, extruded (ISO Data) The addition of PTFE and graphite provides higher wear resistance and lower coefficient of friction compared to the unfilled grade as well as a lower tendency to stick-slip. Duratron T4301 PAI also .. |
|||
Volume Resistivity | >= 1.0e+13 ohm-cm | >= 1.0e+13 ohm-cm | IEC 60093 |
Quadrant EPP Duratron® PAI T4501 PAI + graphite + PTFE, compression moulded (ISO Data) Compression moulded Duratron T4501 PAI is similar in composition to Duratron T4301 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C.. |
|||
Volume Resistivity | >= 1.0e+13 ohm-cm | >= 1.0e+13 ohm-cm | IEC 60093 |
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data) This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica.. |
|||
Volume Resistivity | >= 1.0e+13 ohm-cm | >= 1.0e+13 ohm-cm | IEC 60093 |
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data) Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig.. |