Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 - 1.00e+17 ohm-cm
1.00e+16 - 1.00e+17 ohm-cm
IEC 60093
Raschig Group DECAL® 2061 Phenolic
Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and ..
Volume Resistivity 1.00e+16 - 1.00e+17 ohm-cm
1.00e+16 - 1.00e+17 ohm-cm
IEC 60093
Raschig Group DECAL® 5431 Phenolic
Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/..