Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.060 ohm-cm | 0.060 ohm-cm | |
P & P Technology MS-N Nickel Graphite Conductive Adhesive P & P Technology conductive nickel/graphite adhesive is a one part electrically conductive room temperature curing elastomer. It is supplied as a readily extrudable paste that cures rapidly when exp.. |
|||
Volume Resistivity | 0.060 ohm-cm @Temperature 24.0 °C, Time 3600 sec |
0.060 ohm-cm @Temperature 75.2 °F, Time 1.00 hour |
[ohm/sq], followed by 1 hour at 121°C |
Parker Chomerics CHO-SHIELD® 576 Platable Silver Epoxy Coating Description: CHO-SHIELD® 576 coating is a two component, silver filled, highly conductive epoxy paint designed to provide EMI shielding when applied to a dielectric plastic substrate. This coating .. |
|||
Volume Resistivity | <= 0.060 ohm-cm | <= 0.060 ohm-cm | DC resistance in ohms through a 2.58 cm<sup>2</sup> by 0.02 cm thick sample |
Parker Chomerics CHO-BOND 1029 Conductive Adhesive CHO-BOND® 1029 is a highly conductive silicone adhesive, intended for bonding Chomerics’ conductive silicone EMI gaskets to electrically conductive substrates. It is a two-component, siliver-plate.. |
|||
Volume Resistivity | 0.060 ohm-cm @Temperature 24.0 °C, Time 3600 sec |
0.060 ohm-cm @Temperature 75.2 °F, Time 1.00 hour |
[ohm/sq], followed by 1 hour at 121°C |
Parker Chomerics CHO-SHIELD® 579 Low VOC Silver Epoxy Coating Description: CHO-SHIELD® 579 coating is a two component, silver-filled, highly conductive epoxy paint designed to provide EMI shielding when applied to a dielectric substrate. This coating was spec.. |