Parker Chomerics CHO-SHIELD® 579 Low VOC Silver Epoxy Coating

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Parker Chomerics
Trade Name CHO-SHIELD®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SHIELD® 579 Low VOC Silver Epoxy Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: CHO-SHIELD® 579 coating is a two component, silver-filled, highly conductive epoxy paint designed to provide EMI shielding when applied to a dielectric substrate. This coating was specially developed as a variant of CHO-SHIELD® with a lower VOC rating. CHO-SHIELD® 579 dries to the touch in less than 1 hour at room temperature and attains full chemical resistance after 1 week at room temperature. However, the best electrical properties are achieved by curing at elevated temperatures.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
Electrical Properties Metric English Comments
Volume Resistivity 0.060 ohm-cm

@Temperature 24.0 °C,
Time 3600 sec
0.060 ohm-cm

@Temperature 75.2 °F,
Time 1.00 hour
[ohm/sq], followed by 1 hour at 121°C
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 24.0 °C
1.00 hour

@Temperature 75.2 °F
and 1 hour at 65.5°C, followed by 1 hour at 121°C
60.0 min

@Temperature 24.0 °C
1.00 hour

@Temperature 75.2 °F
and 1 hour at 121°C
60.0 min

@Temperature 24.0 °C
1.00 hour

@Temperature 75.2 °F
and 6 hours at 65.5°C
60.0 min

@Temperature 24.0 °C
1.00 hour

@Temperature 75.2 °F
followed by 4 hours at 79.4°C
Pot Life 480 min
480 min
Shelf Life 9.00 Month
9.00 Month
Descriptive Properties Value Comments
Suggested Spraying Viscosity #2 Zahn Cup 18 - 24 sec
Theoretical Yield 7200 in2/lb