Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | <= 0.038 ohm-cm | <= 0.038 ohm-cm | cured |
Atom Adhesives AA-DUCT 903 Epoxy Adhesive AA-DUCT 903 is an epoxy adhesive and coating formulation based on Nickel. This epoxy nickel formulation offers the maximum continuity of conductivity with an electrical resistivity value of less tha.. |
|||
Volume Resistivity | 0.038 ohm-cm | 0.038 ohm-cm | cured |
Atom Adhesives AA-DUCT N02 Epoxy Adhesive AA-DUCT N02 is a single component, heat curing, conductive epoxy polymer that was designed for ease in handling. This high performance conductive polymer cures quickly at elevated temperatures makin.. |