Polymer Property : Volume Resistivity = 0.0014 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 0.0014 ohm-cm
0.0014 ohm-cm
SGL Carbon Group SIGRAFIL C® C30 T050 EPY Continuous Tow Carbon Fiber with 50k filaments, Epoxy Sizing
SIGRAFIL C as continuous tow is ideal for waving, prepregging, filament winding, Carbon Fiber Reinforced Plastics (CFRP) components, advanced composites, multi-axial production, unidirectional tapes..
Volume Resistivity 0.0014 ohm-cm
0.0014 ohm-cm
Cured: 24 hours at 25°C
Resinlab® SEC1222 Silver Filled Epoxy Adhesive
Resinlab™ SEC1222 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1222 provides excellent electrical conductivit..