Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.0000042 ohm-cm | 0.0000042 ohm-cm | |
H.C. Starck MoCu 80/20 Molybdenum-Copper Composite Material Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t.. |
|||
Volume Resistivity | 0.0000042 ohm-cm | 0.0000042 ohm-cm | |
H.C. Starck MoCu 85/15 Molybdenum-Copper Composite Material Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t.. |