Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 36.0 kV/mm | 914 kV/in | |
LG Chemical AF342 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | |
LG Chemical AF342T ABS, Flame Retardant, High Impact Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | |
Ineos ABS Lustran® H702 Medium heat resistance, increased flow. ,Property data per ISO test methods. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | |
Ineos ABS Triax® 1315 GF ABS + Polyamide Blend (Conditioned) Key Features:Contains FillerSuitable processing methods:Injection molding |
|||
Dielectric Strength | 36.0 kV/mm @Thickness 1.50 mm |
914 kV/in @Thickness 0.0591 in |
Short Time; IEC 60243-1 |
Styrolution Novodur® H702 ABS Novodur H702 is a high heat, high gloss injection molding grade with very good flowabilityInformation provided by Styrolution |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
Vyncolit X7255 Glass Fiber Reinforced Novolac Phenolic Novolac resin based, glass fiber and glass beads reinforced. Very easy to transform in complex shapes. Excellent mechanical and thermal properties. Higher isotropic properties and good dimensional s.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® 2S 25 W 20 HL X black 9992 PA610 Product Description: Grilamid 2S 25 W 20 HL X black 9992 is a semi-flexible high viscosity heat stabilized, impact modified and plasticized Polyamide 610, especially suitable for extrusion applicati.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® 2S 25 W 20 HL X nat PA610 Product Description: Grilamid 2S 25 W 20 HL X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified and plasticized Polyamide 610, espcailly suitable for extrusion applic.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® 2S 25 W 20 HL X nat PA610 Product Description: Grilamid 2S 25 W 20 HL X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified and plasticized Polyamide 610, espcailly suitable for extrusion applic.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4106 black 9992 PA612-GF30 Product description: Grilamid XE 4106 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorpti.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4106 nat PA612-GF30 Product description: Grilamid XE 4106 natural is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorptiong.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 4106 nat PA612-GF30 Product description: Grilamid XE 4106 natural is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorptiong.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4107 black 9992 PA612-GF40 Product description: Grilamid XE 4107 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorpti.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4108 nat PA612-GF50 Product description: Grilamid XE 4108 natural is a 50% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4108 are: low water absorptiong.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4116 black 9288 PA1010-GF55 Product description: Grilamid XE 4116 black 9288 is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, paint.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4116 nat PA1010-GF55 Product description: Grilamid XE 4116 natural is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, painted .. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 4116 nat PA1010-GF55 Product description: Grilamid XE 4116 natural is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, painted .. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
Covestro Makrolon® DP1-1887* Polycarbonate, 10% Glass Filled ISO 7391-PC,MR,(,,)-18-9,GF10Developmental productMVR (300 °C/1.2 kg) 16 cm3/10 min10 % Glass fiber reinforcedMilled fiberLow viscosityEasy releasegood surface qualityInjection molding - Melt tempe.. |
|||
Dielectric Strength | 36.0 kV/mm @Thickness 1.00 mm |
914 kV/in @Thickness 0.0394 in |
ASTM D149 |
Arkema Group Orgalloy® RS 6600 Polyamide 6.6 Alloy Polyamide Alloy, Rigid grade, Nylon 6.6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
BASF Ultraform N 2640 Z6 UNC POM Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
BASF Ultraform® N2320 0035 LEV POM Description: Is a POM, rapidly solidifying standard grade with improved impact strength for injection moldingInformation provided by BASF |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
BASF Ultraform® N2320 U035 POM Description: Is a POM, UV-stabilized injection-molding grade.Information provided by BASF |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | ASTM D149 |
Arlon 51986R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater substrateAppearance: Red colo.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | ASTM D149 |
Arlon 51986RA020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the producti.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
BASF Ultraform® W2320 0035 POM Description: Is a POM, very free-flowing and rapidly solidifying grade for high processing demands.Information provided by BASF |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
Vyncolit W5020 Glass Filled Novolac Phenolic Novolac resin based, glass fiber and glass bead reinforced. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in the ABS system.Inform.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | |
Arkema Group Orgalloy® LT 5050T Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good .. |