EMS-Grivory Grivory® XE 4116 nat PA1010-GF55

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® XE 4116 nat PA1010-GF55.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilamid XE 4116 natural is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, painted parts in complex designs. Grilamid XE 4116 natural has the following product profile: Polymer based primarily on renewable resourcesHigh stiffness and strengthExcellent impact and notched impact strengthImproved warpage performanceImproved flowabilityEasy processingExcellent surface finishGood UV and chemical resistanceImproved paint adhesion Grilamid XE 4116 natural is suitable for the manufacturing of production of moldings in the application fields of: Electronic devicesAutomotive structural partsMechanical engineering, industry goodsSports & leisure goodsInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183
Water Absorption 1.7 %
1.7 %
ISO 62
Moisture Absorption 0.900 %
0.900 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0030 cm/cm
0.0030 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 215 MPa
31200 psi
conditioned; ISO 2039-1
230 MPa
33400 psi
dry; ISO 2039-1
Tensile Strength at Break 180 MPa
26100 psi
conditioned; ISO 527-1/-2
210 MPa
30500 psi
dry; ISO 527-1/-2
Elongation at Break 2.5 %
2.5 %
dry; ISO 527-1/-2
2.5 %
2.5 %
conditioned; ISO 527-1/-2
Tensile Modulus 16.5 GPa
2390 ksi
conditioned; ISO 527-1/-2
17.5 GPa
2540 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
conditioned; ISO 179/1eU
9.00 J/cm²
42.8 ft-lb/in²
dry; ISO 179/1eU
8.00 J/cm²

@Temperature 30.0 °C
38.1 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
8.50 J/cm²

@Temperature 30.0 °C
40.4 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
conditioned; ISO 179/1eA
2.00 J/cm²
9.52 ft-lb/in²
dry; ISO 179/1eA
1.40 J/cm²

@Temperature 30.0 °C
6.66 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
1.50 J/cm²

@Temperature 30.0 °C
7.14 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
5.56 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 °C
212 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 185 °C
365 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 150 °C
302 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
dry; IEC 60093
1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 36.0 kV/mm
914 kV/in
dry; IEC 60243-1
36.0 kV/mm
914 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Compressed air systems
Exterior
Hydraulic systems
Interior
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Lighting
Mobile phones and other portable devices
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Medical devices
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Bio based Polyamide
Improved flowability and demoulding
Special Characteristics High impact or impact modified
Improved UV resistance (outdoor use)