Electrical Properties Metric English Comments
Dielectric Strength 9.10 kV/mm
231 kV/in
Step-by-Step; ASTM D149
Plenco Valite 424 Novolac Phenolic, Granular, Injection Molded  (discontinued **)
This Valite product has been replaced by Plenco 2424. Data provided by Plenco.VALITE 424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a ..
Dielectric Strength 9.10 kV/mm

@Thickness 2.54 mm
231 kV/in

@Thickness 0.100 in
DC
MarkeTech Aluminum Oxide Ceramic - Alumina 96%
Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture..
Dielectric Strength 9.10 kV/mm

@Thickness 2.50 mm
231 kV/in

@Thickness 0.0984 in
DC @ 0.100 in (2.5 mm) thickness
MarkeTech Aluminum Oxide Ceramic - Alumina 97.5%
Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture..
Dielectric Strength 9.10 kV/mm
231 kV/in
ICE Al2O3 94
Data provided by the manufacturer, International Ceramic Engineering.
Dielectric Strength 9.10 kV/mm
231 kV/in
ICE Al2O3 96
Data provided by the manufacturer, International Ceramic Engineering.
Dielectric Strength 9.10 kV/mm
231 kV/in
ICE Al2O3 99.5
Data provided by the manufacturer, International Ceramic Engineering.
Dielectric Strength 9.10 kV/mm
231 kV/in
ICE Al2O3 99.8
Data provided by the manufacturer, International Ceramic Engineering.
Dielectric Strength 9.10 kV/mm
231 kV/in
Short Time; ASTM D149
Plenco 5482 Phenolic, Granular, Injection Molded
PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for elect..
Dielectric Strength 9.10 kV/mm
231 kV/in
Du-Co Ceramics DC-16-L-3 Steatite
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
Dielectric Strength 9.10 kV/mm
231 kV/in
Du-Co Ceramics DC-200-L-5 Fosterite
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
Dielectric Strength 9.10 kV/mm
231 kV/in
Du-Co Ceramics DC-9-L-3 Steatite
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
Dielectric Strength 9.10 kV/mm
231 kV/in
ASTM D149
Chang Chun Plastic Longlite PM T308J General Purpose Phenolic Molding Compound
ASTM Grade per ASTM D700 is 3.Information provided by Dowell Trading Company Ltd.
Dielectric Strength 9.10 kV/mm
231 kV/in
ASTM D149
Chang Chun Plastic Longlite PM T359J General Purpose Phenolic Molding Compound
ASTM Grades per ASTM D700 are 3, 14.Information provided by Dowell Trading Company Ltd.
Dielectric Strength 9.10 kV/mm
231 kV/in
Short Time; Dry; ASTM D149
Resinoid 1329 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance