Resinoid 1329 Phenolic Molding, Glass Reinforced

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Glass Filled
Manufacturer Resinoid
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resinoid 1329 Phenolic Molding, Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Physical Properties Metric English Comments
Density 2.00 g/cc
0.0723 lb/in³
ASTM D792A
Water Absorption <= 0.10 %
<= 0.10 %
24 hours R.T. ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Positive Mold; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D651
Flexural Strength 77.0 MPa
11200 psi
ASTM D790
Flexural Modulus 16.0 GPa
2320 ksi
ASTM D790
Compressive Strength 175 MPa
25400 psi
ASTM D695
Izod Impact, Notched 0.368 J/cm
0.689 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 9.10 kV/mm
231 kV/in
Short Time; Dry; ASTM D149
Arc Resistance 190 sec
190 sec
ASTM D495
Processing Properties Metric English Comments
Mold Temperature 155 - 180 °C
311 - 356 °F