Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 29.7 kV/mm @Thickness 0.800 mm |
754 kV/in @Thickness 0.0315 in |
in oil; ASTM D149 |
SABIC Innovative Plastics LNP THERMOCOMP UF0067W PPA LNP* THERMOCOMP* UF0067W is a compound based on Polyphthalamide resin containing 30% glass fiber. Added features of this material include: Hot Water Moldable, Non-Brominated & Non-Chlorinated Flam.. |