Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.7 - 29.5 kV/mm | 450 - 750 kV/in | Average value: 26.1 kV/mm Grade Count:4 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |