Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 28.3 kV/mm | 720 kV/in | ASTM D149 |
ExxonMobil Santoprene® 121-67W175 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for .. |
|||
Dielectric Strength | 28.3 kV/mm @Thickness 2.03 mm |
720 kV/in @Thickness 0.0799 in |
ASTM D149 |
ExxonMobil Santoprene® 151-70W256 Thermoplastic Vulcanizate - Flame Retardant Product Description: A soft, black, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has been designed to meet the Underwriter Laboratories.. |
|||
Dielectric Strength | 28.3 kV/mm | 720 kV/in | ASTM D149 |
Arlon 51586R015E 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production mat.. |
|||
Dielectric Strength | 28.3 kV/mm | 720 kV/in | After 96 hrs @ 96% RH; ASTM D4325 |
3M Scotch™ 23 Rubber Splicing Tape Scotch® Rubber Splicing Tape 23 is a highly conformable, self-fusing EPR (Ethylene Propylene Rubber) based, high voltage splicing tape. It is a non-vulcanizing, shelf-stable tape with excellent ele.. |