Polymer Property : Dielectric Strength = 670 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 26.4 kV/mm
670 kV/in
short term; ASTM D149
Celanese Celanex® 3216 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 3216 is a non-exuding (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch ),15% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties ..
Dielectric Strength 26.4 kV/mm
670 kV/in
short term; ASTM D149
Celanese Celanex® 7716 PBT, 35% Mineral / Glass Reinforced  (Unverified Data**)
Celanex 7716 is a 35% glass/mineral reinforced, non exuding, flame retarded polybutylene terephthlate which has and excellent balance of mechanical properties and processability. Celanex 7716 is wel..
Dielectric Strength 26.4 kV/mm
670 kV/in
ASTM D149
Westlake Plastics Tempalux® 20% GF Polyetherimide
An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad ..
Dielectric Strength 26.4 kV/mm
670 kV/in
In Oil; ASTM D149
Ensinger TECAPEI® 20% Glass Reinforced, made from Ultem® 2200 PEI
TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in..
Dielectric Strength 26.4 kV/mm
670 kV/in
2.03 mm; ASTM D149
ExxonMobil Santoprene® 121-87 Thermoplastic Elastomer
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
Dielectric Strength 26.4 kV/mm
670 kV/in
short term; ASTM D149
Celanese CELANEX 3216 PBT, 15% Glass Reinforced
Celanex 3216 is a non-exuding (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch ),15% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties ..
Dielectric Strength 26.4 kV/mm
670 kV/in
ASTM D149
Arlon 51228R020 Silicone Rubber/Fiberglass Laminate
Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber
Dielectric Strength 26.4 kV/mm
670 kV/in
ASTM D149
Arlon R35928R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: ..
Dielectric Strength 26.4 kV/mm
670 kV/in
short term; ASTM D149
Celanese CELANEX 7716 PBT, 35% Mineral / Glass Reinforced
Celanex 7716 is a 35% glass/mineral reinforced, non exuding, flame retarded polybutylene terephthlate which has and excellent balance of mechanical properties and processability. Celanex 7716 is wel..