Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 26.4 kV/mm | 670 kV/in | ASTM D149 |
Westlake Plastics Tempalux® 20% GF Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad .. |
|||
Dielectric Strength | 26.4 kV/mm | 670 kV/in | In Oil; ASTM D149 |
Ensinger TECAPEI® 20% Glass Reinforced, made from Ultem® 2200 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
Dielectric Strength | 26.4 kV/mm | 670 kV/in | 2.03 mm; ASTM D149 |
ExxonMobil Santoprene® 121-87 Thermoplastic Elastomer A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Dielectric Strength | 26.4 kV/mm | 670 kV/in | ASTM D149 |
Arlon 51228R020 Silicone Rubber/Fiberglass Laminate Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber |
|||
Dielectric Strength | 26.4 kV/mm | 670 kV/in | ASTM D149 |
Arlon R35928R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: .. |