Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 2.60 kV/mm | 66.0 kV/in | ASTM D149 |
3M Dyneon™ TFM™ 1600 Modified PTFE Powder
(discontinued **) Type III, gr. 2 PTFE. Dyneon TFM 1600 PTFE is a free-flowing powder for compression molding, isostatic molding, automatic molding, and ram extrusion. Dyneon™ TFM™ 1600 PTFE is a second-generatio.. |
|||
Dielectric Strength | 2.60 kV/mm @Thickness 3.17 mm |
66.0 kV/in @Thickness 0.125 in |
Unconditioned; ASTM D149 |
Garlock 9518 Fluoroelastomer Sheet Rubber Gasketing Fluoroelastomer (FKM) Type AExceptional resistance to heat, oils, fuels, numerous acids, and many other chemicals.Information provided by Garlock Rubber Technologies |
|||
Dielectric Strength | 2.60 - 25.0 kV/mm | 66.0 - 635 kV/in | Average value: 23.1 kV/mm Grade Count:51 |
Overview of materials for Thermoset Fluoroelastomer This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr.. |