Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 23.5 kV/mm | 597 kV/in | ASTM D149 |
Saint-Gobain Meldin® 7001 Direct Formed Polyimide Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high .. |
|||
Dielectric Strength | 23.5 kV/mm | 597 kV/in | Arlon SQA-TMS-020 |
Arlon T2030-R004-12 0.030" Cured Self-Fusing Silicone Rubber Tape 1 inch wide, 30 mil thick, 12.0 yards long, red, triangular cross-section, self-fusing silicone tape.Design/Construction:Interleave: 1 mil PETProduct: Cured Silicone Self-fusing RubberCross-section.. |