Arlon T2030-R004-12 0.030" Cured Self-Fusing Silicone Rubber Tape

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon T2030-R004-12 0.030" Cured Self-Fusing Silicone Rubber Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
1 inch wide, 30 mil thick, 12.0 yards long, red, triangular cross-section, self-fusing silicone tape.Design/Construction:Interleave: 1 mil PETProduct: Cured Silicone Self-fusing RubberCross-section: TriangularThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
Silicone Property; Arlon SQA-TMS-024
Water Absorption 0.10 %
0.10 %
Arlon SQA-TMS-016
Thickness 762 microns
30.0 mil
Rubber; Arlon SQA-TMS-012
Mechanical Properties Metric English Comments
Hardness, Shore A 48
48
Silicone Property; Arlon SQA-TMS-014
Tensile Strength 8.391 MPa
1217 psi
Silicone Property; Arlon SQA-TMS-009
Elongation at Break 706 %
706 %
Silicone Property; Arlon SQA-TMS-009
Tear Strength 23.7 kN/m
135 pli
Silicone Property; Arlon SQA-TMS-029
Peel Strength 0.526 kN/m
3.00 pli
Bond Strength; Arlon SQA-TMS-015
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 23.5 kV/mm
597 kV/in
Arlon SQA-TMS-020
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Red