Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 59.0 kV/mm @Temperature 23.0 °C |
1500 kV/in @Temperature 73.4 °F |
in oil, short time. 0.25mm; ASTM D149-97a Method A |
SABIC Innovative Plastics Lexan® FR66 Polycarbonate Film, Flame Retardant Lexan FR66 flame-retardant film is a clear, thin-gauge polycarbonate film with a suede finish on one side and a matte finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Dielectric Strength | 59.0 kV/mm @Temperature 23.0 °C |
1500 kV/in @Temperature 73.4 °F |
in oil, short time. 0.25mm; ASTM D149-97a Method A |
SABIC Innovative Plastics Lexan® FR700 Polycarbonate Film, Flame Retardant Lexan FR700 is a black, one side fine matt, one side velvet flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good d.. |
|||
Dielectric Strength | 59.0 kV/mm @Temperature 23.0 °C |
1500 kV/in @Temperature 73.4 °F |
in oil, short time. 0.25mm; ASTM D149-97a Method A |
SABIC Innovative Plastics Lexan® FR83 Polycarbonate Film, Flame Retardant Lexan* FR83 flame-retardant film is a matt/polished, thin-gauge polycarbonate film with a UL94 VTM-0 listing to meet the stringent requirements in a wide range of electrical, electronic and transpor.. |
|||
Dielectric Strength | 59.0 kV/mm @Temperature 23.0 °C |
1500 kV/in @Temperature 73.4 °F |
in oil, short time. 0.25mm; ASTM D149-97a Method A |
SABIC Innovative Plastics Lexan® FR60 Polycarbonate Film, Flame Retardant Lexan FR60 flame-retardant film is a clear, thin-gauge polycarbonate film with polished surfaces on both sides, and a UL94 V-0 listing to meet the stringent requirements in a wide range of electrica.. |
|||
Dielectric Strength | 59.0 kV/mm @Temperature 23.0 °C |
1500 kV/in @Temperature 73.4 °F |
in oil, short time. 0.25mm; ASTM D149-97a Method A |
SABIC Innovative Plastics Lexan® FR63 Polycarbonate Film, Flame Retardant Lexan FR63 flame-retardant film is a clear, thin-gauge polycarbonate film with a matte finish on one side and a polish finish on the other and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Dielectric Strength | 59.0 kV/mm | 1500 kV/in | |
Von Roll Isola IMI MICA MAT® Inorganic Bonded Mica Plate Data provided by Von Roll Isola USA.Rigid plate designed for use as a non-conducting structural component up to 760°C. 100% inorganic so it maintains good physical and electrical properties at ele.. |
|||
Dielectric Strength | 59.0 kV/mm | 1500 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 418 Paper, 14 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Dielectric Strength | 59.0 kV/mm @Temperature 23.0 °C |
1500 kV/in @Temperature 73.4 °F |
in oil, short time. 0.25mm; ASTM D149-97a Method A |
SABIC Innovative Plastics Lexan® FR65 Polycarbonate Film, Flame Retardant Lexan FR65 flame-retardant film is a clear, thin-gauge polycarbonate film with a velvet finish on one side and a matt finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |