Electrical Properties Metric English Comments
Dielectric Strength 54.0 kV/mm

@Thickness 0.800 mm
1370 kV/in

@Thickness 0.0315 in
in air; ASTM D149
SABIC Innovative Plastics EXTEM UH1006 TPI Blend
High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha..
Dielectric Strength 54.0 kV/mm

@Thickness 0.800 mm
1370 kV/in

@Thickness 0.0315 in
in air; ASTM D149
SABIC Innovative Plastics EXTEM UH1026 TPI Blend
High heat amorphous TPI Blend, Chemical Resistant, High Flow, IR-Transparent
Dielectric Strength 54.0 kV/mm
1370 kV/in
Momentive Performance Materials HBC Hot-Pressed Boron Nitride
Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom..