Dielectric Strength 48.23 kV/mm

@Thickness 0.650 mm
1225 kV/in

@Thickness 0.0256 in
ASTM D149
Lord Adhesives Thermosetâ„¢ EP-830 Ignition Coil Impregnating and Encapsulation Epoxy
Lord EP-830 is a heat curing, two component epoxy formulation designed especially for use in automotive high voltage ignition coils where adhesion to segmented bobbins is critical. The combination o..