Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 48.23 kV/mm @Thickness 0.650 mm |
1225 kV/in @Thickness 0.0256 in |
ASTM D149 |
Lord Adhesives Thermosetâ„¢ EP-830 Ignition Coil Impregnating and Encapsulation Epoxy Lord EP-830 is a heat curing, two component epoxy formulation designed especially for use in automotive high voltage ignition coils where adhesion to segmented bobbins is critical. The combination o.. |