Electrical Properties Metric English Comments
Dielectric Strength 40.0 - 157 kV/mm
1020 - 4000 kV/in
Average value: 81.5 kV/mm Grade Count:5
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..