Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 13.4 - 138 kV/mm | 340 - 3500 kV/in | Average value: 37.9 kV/mm Grade Count:51 |
Overview of materials for Thermoset Polyurethane, Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values .. |