Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 34.6 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 34.6 kV/mm
880 kV/in
ASTM D149
Teknor Apex APEX® 80853-C Polyvinyl Chloride, Flexible
Notes: 105°C, Non-lead Stabilized, Insulation; PVC Insulation intended for use in 90°C wet locations; RoHS CompliantFeatures: Flame Retardant; Oil Resistant Uses: Insulation; Wet Rated Insulat..
Copyright © lookpolymers.com All Rights Reserved