Teknor Apex APEX® 80853-C Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 80853-C Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 105°C, Non-lead Stabilized, Insulation; PVC Insulation intended for use in 90°C wet locations; RoHS CompliantFeatures: Flame Retardant; Oil Resistant Uses: Insulation; Wet Rated Insulation; Wire and Cable ApplicationsAgency Ratings: UL I Oil Rating; UL QMTT2 .E73402 Forms: Pellets Wire Types: MTW; THW-2; TW; THHN; THWN; THW; THWN-2Information Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 71
71
10 seconds; ASTM D2240
Tensile Strength at Break 21.4 MPa
3100 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Continuous Use; ASTM D794
Brittleness Temperature -19.0 °C
-2.20 °F
ASTM D746
Oxygen Index 27 %
27 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 3.40e+15 ohm-cm
3.40e+15 ohm-cm
ASTM D257
3.39e+14 ohm-cm

@Temperature 50.0 °C
3.39e+14 ohm-cm

@Temperature 122 °F
ASTM D257
2.70e+15 ohm-cm

@Temperature 23.0 °C
2.70e+15 ohm-cm

@Temperature 73.4 °F
ASTM D257
Dielectric Constant 2.99

@Frequency 1.00e+6 Hz
2.99

@Frequency 1.00e+6 Hz
ASTM D150
4.36

@Frequency 1000 Hz
4.36

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 34.6 kV/mm
880 kV/in
ASTM D149
Dissipation Factor 0.058

@Frequency 1.00e+6 Hz
0.058

@Frequency 1.00e+6 Hz
ASTM D150
0.095

@Frequency 1000 Hz
0.095

@Frequency 1000 Hz
ASTM D150
Descriptive Properties Value Comments
Appearance Opaque