Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 11.8504 - 12.5197 kV/mm

@Temperature 121 - 121 °C
300.999 - 317.999 kV/in

@Temperature 250 - 250 °F
Average value: 12.2 kV/mm Grade Count:2
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..
Dielectric Strength 11.8504 - 12.5197 kV/mm

@Time 10800 - 10800 sec
300.999 - 317.999 kV/in

@Time 3.00 - 3.00 hour
Average value: 12.2 kV/mm Grade Count:2
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..