Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 11.8504 - 12.5197 kV/mm @Temperature 121 - 121 °C |
300.999 - 317.999 kV/in @Temperature 250 - 250 °F |
Average value: 12.2 kV/mm Grade Count:2 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Dielectric Strength | 11.8504 - 12.5197 kV/mm @Time 10800 - 10800 sec |
300.999 - 317.999 kV/in @Time 3.00 - 3.00 hour |
Average value: 12.2 kV/mm Grade Count:2 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |