Polymer Property : Dielectric Strength = 3100 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 39.0 - 122 kV/mm
991 - 3100 kV/in
Average value: 78.8 kV/mm Grade Count:6
Overview of materials for Solventless Epoxy Varnish, Electrical Insulation
This property data is a summary of similar materials in the MatWeb database for the category "Solventless Epoxy Varnish, Electrical Insulation". Each property range of values reported is minimum and..