Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 31.3 kV/mm | 795 kV/in | |
Tokuyama Shapalâ„¢ SH-15 Sintered Aluminum Nitride Uniform, large sized pressed sintered aluminum nitride. |
|||
Dielectric Strength | 31.3 kV/mm | 794 kV/in | ASTM D149 |
Arlon 32090R028 Silicone Rubber Laminate The interleave is 3 mil polyethylene, side 1 is uncured silicone rubber and the carrier is PET. |