Category Ceramic , Nitride
Manufacturer Tokuyama
Trade Name Shapal™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tokuyama Shapal™ SH-15 Sintered Aluminum Nitride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uniform, large sized pressed sintered aluminum nitride.
Physical Properties Metric English Comments
Density 3.33 g/cc
0.120 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 322 GPa
46700 ksi
Flexural Strength 357 MPa
51800 psi
Poissons Ratio 0.24
0.24
Shear Modulus 130 GPa
18900 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 4.30 µm/m-°C
2.39 µin/in-°F
Thermal Conductivity 159 W/m-K

@Temperature 70.0 °C
1100 BTU-in/hr-ft²-°F

@Temperature 158 °F
184 W/m-K

@Temperature 20.0 °C
1280 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.01e+16 ohm-cm
1.01e+16 ohm-cm
Dielectric Constant 9.1

@Frequency 1.00e+6 Hz
9.1

@Frequency 1.00e+6 Hz
Dielectric Strength 31.3 kV/mm
795 kV/in
Dissipation Factor 0.00030

@Frequency 1.00e+6 Hz
0.00030

@Frequency 1.00e+6 Hz
Descriptive Properties Value Comments
Purity > 94.0 (Al + N)
> 94.8 (Al + N + O)