Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 12.11 kV/mm | 307.7 kV/in | |
Parker Chomerics T-Wing™ Heat Spreader Chomerics family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are not appropriate. T-Wing spreaders consist of.. |