Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 30.7 kV/mm @Thickness 0.510 mm |
780 kV/in @Thickness 0.0201 in |
Z Direction; IPC-TM-650 2.5.6.2 |
Rogers Corporation RO4003C Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil RO4000® Series High Frequency Circuit Materials are glass-reinforced hydrocarbon and ceramic (not PTFE) laminates with TICER™ TCR® Thin Film Resistor Foils. These laminates are designed for perf.. |
|||
Dielectric Strength | 30.7 kV/mm @Thickness 0.510 mm |
780 kV/in @Thickness 0.0201 in |
Z Direction; IPC-TM-650 2.5.6.2 |
Rogers Corporation RO4350B Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil RO4000® Series High Frequency Circuit Materials are glass-reinforced hydrocarbon and ceramic (not PTFE) laminates with TICER™ TCR® Thin Film Resistor Foils. These laminates are designed for perf.. |
|||
Dielectric Strength | 30.7 kV/mm | 780 kV/in | 2.03 mm; ASTM D149 |
ExxonMobil Santoprene® 103-50 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Dielectric Strength | 30.7 kV/mm | 780 kV/in | ASTM D149 |
Arlon LW202R##-P0 0.020" (0.508 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 2 inch wide, 20 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length i.. |
|||
Dielectric Strength | 30.7 kV/mm | 780 kV/in | ASTM D149 |
Arlon 55141R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: uncured silicone rubber; Substrate: 162 fiberglass; Side 2: uncured silicone rubber; Interleave 2: 3 mil PE |
|||
Dielectric Strength | 30.7 kV/mm | 780 kV/in | ASTM D149 |
Arlon 910-10W##-P0 0.010" (0.254 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 10 mil thick, White, Rectangular cross-section, Self-fu.. |
|||
Dielectric Strength | 30.7 kV/mm | 780 kV/in | Arlon SQA-TMS-020 |
Arlon 44580R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass (Flexible Heater Substrate)This data represents typical values for the producti.. |