Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 11.1 kV/mm | 282 kV/in | Step by Step; ASTM D149 |
Plenco 1586 Polyester, Pellet, Injection Molded PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | Short Time; ASTM D149 |
Plenco 4349 Phenolic, Granular, Transfer Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | Short Time; ASTM D149 |
Plenco 7500 Phenolic, Granular, Transfer Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M QI-18/57-325 Cold Shrink Quick Insulator 3M™ Cold Shrink Quick Insulator QI Series are open-ended tubular rubber sleeves with sealing mastic on each end that are factory expanded and assembled onto a removable core. The core is removed by.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M SJ-3A Cold Shrink Jacket Kits 3M™ SJ series Cold Shrink™ Splice Jacket Kits are a series of open ended, tubular, rubber sleeves that combined with Scotch™ 2228 Rubber Mastic Tape provide a sealed jacket over cable splice inst.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | Short Time |
Bulk Molding Compounds BMC SLC 1000 Glass Reinforced Polyester BMC SLC 1000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. It is V-0 flame arc and track resistant. UL® recognized. This material was formerly known.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M 8420-6 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M 8424-8 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M 8425-8 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M 8427-12 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M 8427-6 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M 8428-12 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M 8429-18 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M 8429-6 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M 8430-18 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M 8430-9 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days in water at 90°C; ASTM D149-75 |
3M 8452 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days in water at 90°C; ASTM D149-75 |
3M 8454 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days in water at 90°C; ASTM D149-75 |
3M 8459 Shield Adapter Kit 3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Ki.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days in water at 90°C; ASTM D149-75 |
3M 8460 Shield Adapter Kit 3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Ki.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days in water at 90°C; ASTM D149-75 |
3M 8462 Shield Adapter Kit 3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Ki.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M QI-10/37-270 Cold Shrink Quick Insulator 3M™ Cold Shrink Quick Insulator QI Series are open-ended tubular rubber sleeves with sealing mastic on each end that are factory expanded and assembled onto a removable core. The core is removed by.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M QSLV-M-2-500 Cold Shrink Quick Splice Low Voltage 3M™ Cold Shrink Quick Splice Low Voltage QSLV-M are open-ended tubular rubber sleeves with sealing mastic on each end which are factory expanded and assembled onto a unique three-core system. Two c.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M QSLV-M-8-2/0 Cold Shrink Quick Splice Low Voltage 3M™ Cold Shrink Quick Splice Low Voltage QSLV-M are open-ended tubular rubber sleeves with sealing mastic on each end which are factory expanded and assembled onto a unique three-core system. Two c.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M SJ-1A Cold Shrink Jacket Kits 3M™ SJ series Cold Shrink™ Splice Jacket Kits are a series of open ended, tubular, rubber sleeves that combined with Scotch™ 2228 Rubber Mastic Tape provide a sealed jacket over cable splice inst.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M 8426-9 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M 8427-16 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M 8429-9 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | 7 days in water at 90°C; ASTM D149-75 |
3M 8461 Shield Adapter Kit 3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Ki.. |
|||
Dielectric Strength | 11.1 kV/mm | 282 kV/in | Short Time; ASTM D149 |
Plenco 7307 Phenolic, Granular, Transfer Molded PLENCO 07307 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength properties. Type ASTM 5948 CFG, and UL recognized under component file E40654. 07307 is a.. |