Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 25.1 - 26.2 kV/mm | 638 - 665 kV/in | DC Breakdown Strength |
China-Yixing Longly Refractories ZTA (20%ZrO2) Zirconia Toughened Alumina Composite Ceramic LONGLY's Zirconia Toughened Alumina ceramics (hereafter referred as composite ceramic, ZTA) is white, corrosion resistance, good chemical stability. As well all know that alumina is hard, while zir.. |
|||
Dielectric Strength | 25.1 kV/mm | 638 kV/in | ASTM D149 |
Arlon 55576R060 0.060" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |