Electrical Properties Metric English Comments
Dielectric Strength 23.2 kV/mm
590 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® PBT WM35 X
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Dielectric Strength 23.2 kV/mm
590 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® PBT GF/M40 BK 40% Glass/Mineral Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Dielectric Strength 23.2 kV/mm
590 kV/in
ASTM D149
Arlon 55572AA024 0.024" (0.610 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass This data represents typical values for the production material. The data should not be us..
Dielectric Strength 23.2 kV/mm
590 kV/in
ASTM D149
Arlon 55106R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber
Dielectric Strength 23.2 kV/mm
590 kV/in
ASTM D149
Arlon 55146R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber