Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® PBT GF/M40 BK 40% Glass/Mineral Filler

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass + Mineral Filled
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PBT GF/M40 BK 40% Glass/Mineral Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
ASTM D792
Water Absorption 0.070 %

@Time 86400 sec
0.070 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ASTM D785
Tensile Strength, Yield 75.8 MPa
11000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 7.93 GPa
1150 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm

@Thickness 3.17 mm
1.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.2 µm/m-°C
14.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 199 °C
390 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+15 ohm-cm
3.00e+15 ohm-cm
ASTM D257
Dielectric Strength 23.2 kV/mm
590 kV/in
Method A (Short-Time); ASTM D149