Polymer Property : Dielectric Strength = 23 kV/mm
Polymer Property :
Dielectric Strength =
23 kV/mm
Product List
Electrical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties
Metric
English
Comments
Dielectric Strength
23
kV/mm
580
kV/in
Short Term; ASTM D149
Quadrant EPP Semitron® CMP XL20 (ASTM Product Data Sheet)