Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 21.4 kV/mm | 544 kV/in | ASTM D149 |
CPC - Vycom VINTEC I® PVC Polyvinyl Chloride (PVC) Vintec I is a normal impact, high corrosion resistant polyvinyl chloride (PVC) sheet. Because of its exceptional corrosion resistance, it is ideally suited for applications where maximum chemical re.. |
|||
Dielectric Strength | 21.4 kV/mm | 543 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M 8440 Silicone Rubber Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators 8440 Series are open ended, silicone rubber, tubular sleeves. The sleeves are factory expanded and assembled on a removable supporting plastic core. Each rubber.. |
|||
Dielectric Strength | 21.4 kV/mm | 544 kV/in | ASTM D149 |
CPC - Vycom Ultra White™ PVC Advanced, UV (Ultra Violet) resistant sheet Ultra White is an advanced PVC formulation designed specifically for outdoor applications where resistance to ultraviolet (UV) degradation is critical. Tests show that Ultra White retards both surfa.. |