Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 206 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 8.10 kV/mm
206 kV/in
AC 60 Hz; 150°C for 1,000 hrs
Fujipoly Industries Sarcon® 45H Thin-Film HR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Strength 8.10 kV/mm
206 kV/in
Short Time; ASTM D149
Plenco 7556 Phenolic, Briquette, Transfer Molded
PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component..
Copyright © lookpolymers.com All Rights Reserved