Electrical Properties Metric English Comments
Dielectric Strength 2.61 kV/mm
66.3 kV/in
Short Time; ASTM D149
Plenco 08133 Polyester BMC, Compression Molded
PLENCO 08133 is a renumber of PlasGlas 10313. PLENCO 08133 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co..