Electrical Properties Metric English Comments
Dielectric Strength 2.50 - 165 kV/mm
63.5 - 4200 kV/in
Average value: 57.8 kV/mm Grade Count:65
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v..
Dielectric Strength 2.50 kV/mm
63.5 kV/in
ASTM D149
3M Dyneon™ 1620 PTFE Powder  (discontinued **)
Type II, gr. 3 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
Dielectric Strength 2.50 kV/mm
63.5 kV/in
ASTM D149
3M Dyneon™ 1641 PTFE Powder  (discontinued **)
Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
Dielectric Strength 2.50 kV/mm
63.5 kV/in
ASTM D149
3M Dyneon™ 1645 PTFE Powder  (discontinued **)
Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
Dielectric Strength 2.50 kV/mm
63.5 kV/in
200°C for 1,000 hrs
Fujipoly Industries Sarcon® 15GHR Thin-Film GHR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Strength 2.50 kV/mm
63.5 kV/in
60°C for 500 hrs
Fujipoly Industries Sarcon® 15GHR Thin-Film GHR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Strength 2.50 kV/mm
63.5 kV/in
ASTM D149-95a
3M Dyneon™ TF 1620 PTFE
Meets ASTM D4894 Type IV, Grade 2 resinSemi-free-flowing compression molding powderHigh bulk densityGood for large billets and thin walled isostatic moldingsVery dense polymer structure, similar to ..