Electrical Properties Metric English Comments
Dielectric Strength 2.50 - 165 kV/mm
63.5 - 4200 kV/in
Average value: 57.8 kV/mm Grade Count:65
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v..